exclusion

CROMAROD® DUPLEX

CROMAROD® DUPLEX is a rutile flux coated electrode which deposits a 24%Cr / 10%Ni / 3%Mo / 0.15%N austenitic-ferritic duplex stainless steel weld metal having a ferrite content of about FN 35. The electrode is easy to use and p roduces a smooth weld bead finish and good slag  detachability.  CROMAROD® DUPLEX is designed for …

CROMAROD® DUPLEX B

CROMAROD® DUPLEX B is a basic flux coated electrode intended for welding similar composition duplex stainless steels e.g. 1.4462, UNS 31803. The basic coating design produces a very low micro-oxide level in the deposit, giving excellent fracture toughness at temperatures down to -46 °C. Duplex stainless steels offer an excellent combination of high strength and …

CROMAROD® DUPLEX LP

CROMAROD® DUPLEX LP is a fully positional rutile flux coated electrode designed specially for pipe-welding. It has a thin coating and fast-frezing slag, making it ideal for root runs. The electrode is intended for welding similar composition duplex stainless steels, e.g. 1.4462, UNS 31803. With thicker walled pipe it can be advantageous to use CROMAROD® …

CROMATIG 308H

CROMATIG 308H deposits a 20%Cr-10%Ni austenitic stainless steel weld metal with controlled carbon content (0,04%-0,08%). It is designed to weld similar composition steels, used for their creep strength and oxidation resistance at temperatures up to 800°C. CROMATIG 308H is also recommended for welding the controlled carbon stabilised grades 321H and 347H, used for structural applications …

CROMATIG 308L

CROMATIG 308L is primarily intended for welding the low carbon 18% Cr / 10% Ni, type 304L, austenitic stainless steels. It is also suitable for stainless steel grade 304 material and the Nb or Ti stabilised grades 347 and 321, provided service temperatures for structural applications are below 400°C.

CROMATIG 308LSi

CROMATIG 308LSi is is primarily intended for welding the low carbon 18% Cr / 10% Ni, type 304L, austenitic stainless steels. It is also suitable for stainless steel grade 304 material and the Nb or Ti stabilised grades 347 and 321, provided service temperatures for structural work are below 400°C. The higher silicon content provides a …